Ovako is a leading European producer of engineering steel for customers in the bearing, transportation and manufacturing industries. Our production is based on recycled steel and includes steel in the form of bars, tubes, rings and pre-components.
Headquarters
Stockholm, Sweden
Website
Type
Manufacturer and Processor
Certifications
ISO 45001
, ISO 14001
, ISO 9001
, ISO 50001
Grade | Shape | ||
---|---|---|---|
EN 16MnCr5 | Bar | EN 16MnCr5, EN 20MnCr5 | |
EN 16NiCrS4 | Bar | EN 16NiCrS4 | |
EN 18CrNiMo7-6 | Bar | EN 18CrNiMo7-6, DIN 1.6587, AISI 4820, DIN 17CrNiMo6, AFNOR 18CND6 | EN ISO 683-3, EN ISO 683-17 |
EN 20NiCrMo2-2 | Bar | EN 20NiCrMo2-2, SAE 8620, BS 805H22, AFNOR 20NCD2, SS 2506 | |
EN C15E | Bar | EN C15E | |
Ovaco 677 | Bar | EN 67SiMnCrMo6-6-4, EN 66SiMnCrMo6-6-4 | |
Ovako 124 | Tube | EN 20MoCr4 | EN 10084 |
Ovako 146 | Bar | EN 16NiCrMo7-8 | |
Ovako 152 | Bar | EN 20NiCrMo2-2, AISI 8620, AISI 8620H, DIN 1.6522, DIN 1.6523, DIN 1.6526, SS 2506, UNS H86200 | EN ISO 683-3 |
Ovako 157 | Bar | EN 20NiCrMo7, ASTM 4320, ASTM 4320H | |