About Slovalco

Slovalco is primary aluminium producer. Our final products are aluminium alloys in the shape of extrusion ingots and primary foundry alloys shaped as ingots. Aluminium products are further processing in other industries (automotive, aircraft, electro-technical, construction etc.).

Company profile

Headquarters

Žiar nad Hronom, Slovakia

Type

Manufacturer and Processor

Certifications

ISO 9001

, IATF 16949

, IEC 17025

, ISO 17025

, ISO 14001

, ISO 45001

, ISO 27001

, IEC 27001

, ISO 22301

, ISO 50001

, AD 2000

Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

EN Al99.5

Extrusion

EN Al99.5

EN 1676

EN Al99.7

Extrusion

EN Al99.7

EN 1676

EN AlCu4MgTi

Extrusion

EN AlCu4MgTi, EN AB-21000

EN 1676

EN AlCu4Ti

Extrusion

EN AlCu4Ti, EN AB-21100

EN 1676

EN AlSi10Mg(A)

Extrusion

EN AlSi10Mg(A), EN AB-43000

EN 1676

EN AlSi11

Extrusion

EN AlSi11, EN AB-44000

EN 1676

EN AlSi12(A)

Extrusion

EN AlSi12(A), EN AB-44200

EN 1676

EN AlSi7Mg0.3

Extrusion

EN AlSi7Mg0.3, EN AB-42100

EN 1676

EN AlSi7Mg0.6

Extrusion

EN AlSi7Mg0.6, EN AB-42200

EN 1676

EN AlSi9Cu1Mg

Extrusion

EN AlSi9Cu1Mg, EN AB-46400

EN 1676

Showing 1 to 10 of 11 entries

Previous

1
2

Next

Locations

Slovakia

Slovakia

Priemyselná 14

965 48 Žiar nad Hronom

(+421)456089999