Grade | Shape | ||
---|---|---|---|
AISI 201A | Slab, Strip, Sheet | AISI 201A | |
AISI 202 | Slab, Strip, Sheet | AISI 202 | |
ASTM TP304L | Slab, Strip, Sheet | ASTM TP304L, ASTM MT304, AISI 304L | ASME SA312, ASTM A312, ASTM A554 |
EN 1.4301 | Slab, Strip, Sheet | EN 1.4301, ASTM TP304, ASTM MT304, JIS SUS304, JIS SUS304TP, JIS SUS304TB, JIS SUS304TK, JIS SUS304CSP, AISI 304 | EN 10028-7, EN 10088-2, ASME SA240, ASME SA249, ASME SA312, ASTM A240, ASTM A249, ASTM A312, ASTM A666, ASTM A554, JIS G4304, JIS G4305, JIS G3459, JIS G3463, JIS G4313, JIS G3446 |
EN 1.4307 | Slab, Strip, Sheet | EN 1.4307, ASTM 304L, AISI 304L | EN 10028-7, EN 10088-2, ASME SA240, ASME SA249, ASTM A240, ASTM A249 |
EN 1.4310 | Slab, Strip, Sheet | EN 1.4310, ASTM 301, JIS SUS301, AISI 301 | EN 10088-2, ASME SA240, ASTM A240, JIS G4304, JIS G4305 |
EN 1.4318 | Slab, Strip, Sheet | EN 1.4318, ASTM 301L, JIS SUS301L, AISI 301L | EN 10028-7, EN 10088-2, ASME SA240, ASTM A240, JIS G4304, JIS G4305 |
EN 1.4372 | Slab, Strip, Sheet | EN 1.4372, ASTM 201, AISI 202 | EN 10088-2, ASME SA240, ASME SA249, ASTM A240, ASTM A249 |
JIS SUS304TP | Slab, Strip, Sheet | JIS SUS304TP, JIS SUS304TB, AISI 304 | JIS G4304, JIS G4305, JIS G3459, JIS G3463 |