Established In 1967, Resistaloy Inc. has become a leader among Canadian based Stainless Steel Suppliers, providing Stainless Steel Pipe; Stainless Steel Tubes, Stainless Steel Valves, Fittings, & Pumps for the Chemical, Petro-Chemical, Pulp and Paper, and Mining Industries, as well as food and beverage producers.
Grade | Shape | ||
---|---|---|---|
AISI 309 | Tube, Pipe | AISI 309, AISI 309S | |
ASTM 304 | Tube, Pipe | ASTM 304, ASTM 304L | ASTM A249, ASTM A269, ASTM A270 |
ASTM 310 | Tube, Pipe | ASTM 310, ASTM 310S | |
ASTM 316L | Tube, Pipe | ASTM 316L, ASTM 316 | ASTM A249, ASTM A269, ASTM A270 |
ASTM 317 | Tube, Pipe | ASTM 317, ASTM 317L | |
ASTM 321 | Tube, Pipe | ASTM 321 | |
ASTM 347 | Tube, Pipe | ASTM 347 | |
ASTM 409 | Tube, Pipe | ASTM 409 | |
ASTM 410 | Tube, Pipe | ASTM 410 | ASTM A268 |
ASTM 430 | Tube, Pipe | ASTM 430 | ASTM A268 |