Zwahlen & Mayr is a primary contributor to the international industry and is active in 2 main sectors: -Production of welded stainless steel tubes -Steel construction.
Headquarters
Porcia,Pordenone, Italy
Website
Type
Manufacturer and Processor
Grade | Shape | ||
---|---|---|---|
AL6XN | Tube | AL6XN, UNS N08367 | EN 10217-7, ASTM B676, EN 10357, ASTM A270 |
EN 1.4162 | Tube | EN 1.4162, Alloy 2101, UNS S32101 | EN 10217-7, ASTM A789, EN 10357, ASTM A270 |
EN 1.4301 | Tube | EN 1.4301, AISI 304, EN X5CrNi18-10, EN X4CrNi18-10, UNS S30400 | EN 10217-7, ASTM A249, ASTM A688, EN 10357, ASTM A270 |
EN 1.4306 | Tube | EN 1.4306, AISI 304L, EN X2CrNi19-11, UNS S30403 | EN 10217-7, ASTM A249, ASTM A688, EN 10357, ASTM A270 |
EN 1.4307 | Tube | EN 1.4307, AISI 304L, EN X2CrNi18-9, UNS S30403 | EN 10217-7, ASTM A249, ASTM A688, EN 10357, ASTM A270 |
EN 1.4362 | Tube | EN 1.4362, AISI 2304, EN X2CrNiN23-4, UNS S32304 | EN 10217-7, ASTM A789, EN 10357, ASTM A270 |
EN 1.4401 | Tube | EN 1.4401, AISI 316, EN X5CrNiMo17-12-2, UNS S31600 | EN 10217-7, ASTM A249, ASTM A688, EN 10357, ASTM A270 |
EN 1.4404 | Tube | EN 1.4404, AISI 316L, EN X2CrNiMo17-13-2, EN X2CrNiMo17-12-2, UNS S31603 | EN 10217-7, ASTM A249, ASTM A688, EN 10357, ASTM A270 |
EN 1.4410 | Tube | EN 1.4410, AISI 2507, EN X2CrNiMoN25-7-4, UNS S32750 | EN 10217-7, ASTM A789, EN 10357, ASTM A270 |
EN 1.4432 | Tube | EN 1.4432, AISI 316L, EN X2CrNiMo17-12-3 | EN 10217-7, ASTM A249, ASTM A688, EN 10357, ASTM A270 |