Ceramic Silicon Carbide Composite SICAPRINT™ Si10

Ceramic Silicon Carbide Composite SICAPRINT™ Si100

Ceramic Silicon Carbide Composite SICAPRINT™ Si200

Search results

Materials

Available properties

General

Porosity (%)
Density (g/cm³)

Mechanical

Elastic modulus (GPa)
Flexural strength (MPa)

Thermal

Thermal conductivity (W/(m·K))

Electrical

Electrical resistivity (Ω·m)

You should select at least 1 property to see the chart!

Ceramic Silicon Carbide Composite SICAPRINT™ Si10

Ceramic Silicon Carbide Composite SICAPRINT™ Si100

Ceramic Silicon Carbide Composite SICAPRINT™ Si200

Primary standard name

Equivalent standard names

Related standards

Chemical composition

Element

Weight %

Comment

Element

Weight %

Comment

Element

Weight %

Comment

Material Information

Secondary Phase

Mechanical

Elastic modulus, E

270 GPa at 23 °C

320 GPa at 23 °C

360 GPa at 23 °C

Flexural strength, σbend

110 MPa at 23 °C

150 MPa at 23 °C

180 MPa at 23 °C

General

Porosity, Vvoid

0.1 %

0.1 %

0.1 %

Density, ρ

2.8 g/cm³ at 23 °C

2.9 g/cm³ at 23 °C

3 g/cm³ at 23 °C

Electrical

Electrical resistivity, ρel

7.5E-5 Ω·m at 23 °C

8E-5 Ω·m at 23 °C

8E-5 Ω·m at 23 °C

Thermal

Thermal conductivity, λ

120 W/(m·K) at 23 °C

150 W/(m·K) at 23 °C

170 W/(m·K) at 23 °C