Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Want to keep this datasheet? Save it now in your required format
Description
Here we bring the excellent physical properties of silicon carbide into complex shapes.
The material base and the broad range of refinement processes allow us to produce tough industrial components with high heat resistance, high thermal conductivity and hardness. The different types of SICAPRINT Si give our customers the opportunity to choose the most economical type for their application.
The advantages of SICAPRINT™ Si are:
Temperature stability up to 1400 °C
Excellent thermal conductivity
High hardness
This material data has been provided by SGL Carbon.