Ceramic Silicon Carbide Composite SICAPRINT™ Si100

Want to keep this datasheet? Save it now in your required format

Description

Here we bring the excellent physical properties of silicon carbide into complex shapes.


The material base and the broad range of refinement processes allow us to produce tough industrial components with high heat resistance, high thermal conductivity and hardness. The different types of SICAPRINT Si give our customers the opportunity to choose the most economical type for their application.


The advantages of SICAPRINT™ Si are:

  • Temperature stability up to 1400 °C
  • Excellent thermal conductivity
  • High hardness

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

2.9 g/cm³

Show Supplier Material materials with Density of 2.9 g/cm³

Porosity

0.1 %

Show Supplier Material materials with Porosity of 0.1 %

open porosity, max

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

320 GPa

Show Supplier Material materials with Elastic modulus of 320 GPa

Flexural strength

23.0 °C

150 MPa

Show Supplier Material materials with Flexural strength of 150 MPa

Thermal

PropertyTemperatureValue

Thermal conductivity

23.0 °C

150 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 150 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

8E-5 Ω·m

Show Supplier Material materials with Electrical resistivity of 8E-5 Ω·m