Kohlenstoffarmer Stahl
EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Austenitischer rostfreier Stahl
EN 10028-7 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Kohlenstoffarmer Stahl
EN 10269 Grade 19MnB4 quenched and tempered (+QT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNiTiB18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X3CrNiMoN17-13 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X8CrNiTi18-10 solution annealed (+AT)Kohlenstoffarmer Stahl
EN 10263-4 Grade 19MnB4 annealed to achieve spheroidized carbides (+AC)Kohlenstoffarmer Stahl
EN 10263-4 Grade 19MnB4 annealed to achieve spheroidized carbides and turnedKohlenstoffarmer Stahl
EN 10263-4 Grade 22B2 annealed to achieve spheroidized carbides (+AC)Kohlenstoffarmer Stahl
EN 10263-4 Grade 22B2 annealed to achieve spheroidized carbides and turnedKohlenstoffarmer Stahl
EN 10263-4 Grade 28B2 annealed to achieve spheroidized carbides (+AC)Kohlenstoffarmer Stahl
EN 10263-4 Grade 28B2 annealed to achieve spheroidized carbides and turnedKohlenstoffarmer Stahl
EN 10269 Grade 19MnB4 annealed to achieve spheroidized carbides (+AC)Kohlenstoffarmer Stahl
JIS G3128 Grade E460E normalized, controlled rolledAustenitischer rostfreier Stahl
EN 10216-5 Grade X7CrNiTiB18-10 solution annealed (+AT)Medium Carbon Steel
EN 10269 Grade 35B2 quenched and tempered (+QT)