Elastizitätsmodul: 186.85 GPa

Quick Comparison

Kohlenstoffarmer Stahl

EN 10028-2 Grade P235GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-2 Grade P265GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Austenitischer rostfreier Stahl

DIN 17440 Grade X5CrNiMo17-12-2 quenched (+Q)

Aushärtbarer Stahl

UNS S45500 Annealed