Kohlenstoffarmer Stahl
EN 10025-2 Grade S275J2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-3 Grade P275NH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-3 Grade P275NL1 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-3 Grade P275NL2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S275JR normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S275J0 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade E295 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade E335 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade E360 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-3 Grade S260NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00