spezifischer Widerstand: 2E-7 - 2.16E-7 Ω·m

Quick Comparison

Kohlenstoffarmer Stahl

EN 10028-2 Grade P265GH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-3 Grade P275NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-3 Grade P275NL1 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10028-3 Grade P275NL2 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10149-2 Grade S420MC thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10149-2 Grade S460MC thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10149-2 Grade S500MC thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

EN 10149-2 Grade S550MC thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Chromium Steel

ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00