Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10149-2 Grade S420MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S460MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S500MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S550MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Kohlenstoffarmer Stahl
EN 10217-3 Grade WStE 255 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17179 Grade WStE 255 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10217-3 Grade StE 255 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10217-3 Grade TStE 255 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17125 Grade TStE 255 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17125 Grade StE 255 normalized or normalized formed (+N)Near-Alpha-Legierung
DIN 17850 Grade Ti3Pd AnnealedKohlenstoffarmer Stahl
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Nickel-Kupfer-Legierung
DIN 17743 Grade NiCu30Fe soft annealed (+A)