Ductile (Nodular) Cast Iron
EN 1564 Grade GJS-1200-2 austemperedMartensitischer Edelstahl
ASTM A564 Grade XM-12 H925Martensitischer Edelstahl
ASTM A705 Grade XM-12 Age-Hardening H925Wrought Copper High Copper Alloy
EN 12166 Grade CuBe2Pb H350Martensitischer Edelstahl
ASTM A564 Grade XM-12 H900Martensitischer Edelstahl
ASTM A705 Grade XM-12 Age-Hardening H900Wrought Copper High Copper Alloy
EN 12165 Grade CuBe2 M