Heat deflection temperature, 0.45 MPa: 252 °C

Quick Comparison

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF007ES

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RF206

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF002SXS

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF006ESZ

Geliefert von:

Sabic

Polyethylenterephthalat (PET)

Arnite® AV2 390

Geliefert von:

DSM Engineering Materials

Polyethylenterephthalat (PET)

Arnite® AV2 390 XL

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RC003SXS

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RC003

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RX03643H

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RF206AXH

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00AH

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF006EXZ

Geliefert von:

Sabic