General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Density of 1.19 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 28 % Show Supplier Material materials with Limiting oxygen index of 28 % | |
Water absorption | 23.0 °C | 5.5 % Show Supplier Material materials with Water absorption of 5.5 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 13 GPa Show Supplier Material materials with Elastic modulus of 13 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 10 GPa Show Supplier Material materials with Flexural modulus of 10 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 230 MPa Show Supplier Material materials with Flexural strength of 230 MPa | ISO 178 | break, 2 mm/min |
Hardness, Rockwell L | 23.0 °C | 105 [-] Show Supplier Material materials with Hardness, Rockwell L of 105 [-] | ISO 2039-2 |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 170 MPa Show Supplier Material materials with Tensile strength of 170 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.1E-4 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature | 250 - 252 °C Show Supplier Material materials with Heat deflection temperature of 250 - 252 °C | ||||
Heat deflection temperature, 0.45 MPa | 252 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 252 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 250 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 250 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Vicat softening temperature | 255 °C Show Supplier Material materials with Vicat softening temperature of 255 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Compliant, 94HB Flame Class Rating: 1.6mm UL 94 by SABIC-IP |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 178000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 178000 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 178000 Ω·cm Show Supplier Material materials with Volume resistivity of 178000 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas, Personal Computing, Industrial Material Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 75 to 85.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |