General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 11.2 GPa Show Supplier Material materials with Elastic modulus of 11.2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 2.4 % Show Supplier Material materials with Elongation of 2.4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 9.7 GPa Show Supplier Material materials with Flexural modulus of 9.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 268 MPa Show Supplier Material materials with Flexural strength of 268 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 524 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 524 J/m | ASTM D 4812 | 23°C |
Poisson's ratio | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poisson's ratio of 0.4 [-] | ASTM E 132 |
Tensile strength | 23.0 °C | 197 MPa Show Supplier Material materials with Tensile strength of 197 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100000 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |