Blei: 0 - 2.5 %

Quick Comparison

Unclassified Low Alloy Steel

EN 10225 Grade S420G1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10225 Grade S355G7 thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10225 Grade S420G1 thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10225 Grade S460G1 thermomechanically rolled

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

2000 Serie

AA Standards Grade 2011 T3

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

AA Standards Grade 2011 T8

Geliefert von:

1 Matmatch-Lieferant

Nickel Chromium Iron Alloy

VDM® Alloy 718

Geliefert von:

VDM Metals

2000 Serie

AA Standards Grade 2011 T6

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Nickel-Kupfer-Legierung

VDM® Alloy K-500

Geliefert von:

VDM Metals

2000 Serie

DIN 1725-1 Grade 3.1655 T3

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

DIN 1725-1 Grade 3.1655 T8

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

DIN 1725-1 Grade 3.1655 T8

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

DIN 1725-1 Grade 3.1655 T3

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

AA Standards Grade 2011 T4

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

EN 573-3 Grade AW-2011 T3

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

DIN 1725-1 Grade 3.1645 T3

Geliefert von:

2 Matmatch-Lieferanten

Seite 1 von 254