Duplex rostfreier Stahl
EN 10095 Grade X10NiCrSiNb35-22 solution annealed (+AT)Superaustenitic Stainless Steel
EN 10095 Grade X12NiCrSi35-16 solution annealed (+AT)Superaustenitic Stainless Steel
SEW 470 Grade X12NiCrSi35-16 solution annealed (+AT)Nickel Steel
DIN 17465 Grade GX40NiCrSi38-18 cast conditionSuperaustenitic Stainless Steel
EN 10095 Grade X10NiCrSi35-19 solution annealed (+AT)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr20CuMo stabilizedSuperaustenitic Stainless Steel
DIN 17465 Grade GX40NiCrSiNb38-18 cast conditionNickel Steel
SEW 385 Grade Ni36 soft annealed (+A)Austenitischer rostfreier Stahl
ASTM Alloy 20 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A182 Grade F44 Solution-AnnealedAustenitischer rostfreier Stahl
ASTM A240 Grade S35135 Heat-TreatedNickel Steel
DIN 41301 Grade D3 fully processed