General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 223 GPa Show Material materials with Elastic modulus of 223 GPa | |
100.0 °C | 217 GPa Show Material materials with Elastic modulus of 217 GPa | ||
200.0 °C | 209 GPa Show Material materials with Elastic modulus of 209 GPa | ||
300.0 °C | 201 GPa Show Material materials with Elastic modulus of 201 GPa | ||
400.0 °C | 192 GPa Show Material materials with Elastic modulus of 192 GPa | ||
500.0 °C | 183 GPa Show Material materials with Elastic modulus of 183 GPa | ||
Hardness, Brinell | 20.0 °C | 230 [-] Show Material materials with Hardness, Brinell of 230 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Martensitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa Show Material materials with Shear modulus of 77 GPa | Typical for Martensitic Stainless Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.04E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.04E-5 1/K | |
200.0 °C | 1.08E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K | ||
300.0 °C | 1.12E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.12E-5 1/K | ||
400.0 °C | 1.16E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.16E-5 1/K | ||
500.0 °C | 1.19E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K | ||
Melting point | 1370 - 1530 °C Show Material materials with Melting point of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Specific heat capacity | 20.0 °C | 430 J/(kg·K) Show Material materials with Specific heat capacity of 430 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 15 W/(m·K) Show Material materials with Thermal conductivity of 15 W/(m·K) |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 6E-7 Ω·m Show Material materials with Electrical resistivity of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.25 - 0.35 % Show Material materials with Carbon of 0.25 - 0.35 % |
Chromium | 14 - 16 % Show Material materials with Chromium of 14 - 16 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Molybdenum | 0.85 - 1.1 % Show Material materials with Molybdenum of 0.85 - 1.1 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Nitrogen | 0.3 - 0.5 % Show Material materials with Nitrogen of 0.3 - 0.5 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 1 % Show Material materials with Silicon of 1 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |