Kohlenstoffarmer Stahl
EN 10149-2 Grade S420MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Nickel Steel
EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-5 Grade P460M thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10149-2 Grade S600MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
EN 10083-1 Grade C45E quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C50E quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C50E quenched and tempered (+QT)Medium Carbon Steel
EN 10277-5 Grade C45 cold drawn or turned and quenched and temperedMedium Carbon Steel
EN 10277-5 Grade Ck45 cold drawn or turned and quenched and tempered