The thermomechanical rolled steel S600MC, mat. no. 1.8969, is used for cold formed components like vehicle frames, axles and special sections. Tempering > 580 deg. leads to an decrease of the strength of the thermomechanical treated material. The lowest application temperature amounts to - 20 deg. At this temperature the proof of the notch impact energy of min. 40 J can be agreed. The min. bending mandrel diameter for the 180°-bending test (transversal specimen) amounts to 1,5*t (t=specimen thickness).

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

20.0 °C

11 - 13 %

Show Material materials with Elongation of 11 - 13 %

Elongation A80

20.0 °C

11 - 13 %

Show Material materials with Elongation A80 of 11 - 13 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Tensile strength

20.0 °C

650 - 820 MPa

Show Material materials with Tensile strength of 650 - 820 MPa

Yield strength

20.0 °C

600 MPa

Show Material materials with Yield strength of 600 MPa

Thermal

PropertyValue

Max service temperature, long

-20 - 0 °C

Show Material materials with Max service temperature, long of -20 - 0 °C

Chemical properties

PropertyValue

Aluminium

0.015 %

Show Material materials with Aluminium of 0.015 %

Boron

5E-3 %

Show Material materials with Boron of 5E-3 %

Carbon

0.12 %

Show Material materials with Carbon of 0.12 %

Manganese

1.9 %

Show Material materials with Manganese of 1.9 %

Molybdenum

0.5 %

Show Material materials with Molybdenum of 0.5 %

Niobium

0.09 %

Show Material materials with Niobium of 0.09 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.22 %

Show Material materials with Titanium of 0.22 %

Vanadium

0.2 %

Show Material materials with Vanadium of 0.2 %