Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J2C normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355K2C normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S460MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-2 Grade S500MC thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
7000 Serie
AA Standards Grade 7075 T7351Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Unclassified Low Alloy Steel
EN 10025-6 Grade S550QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S620QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-3 Grade S460N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-3 Grade S460NL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S460ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-6 Grade S500Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-6 Grade S500QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QL2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P460Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant