Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | ||||
Elongation | 13.8 % Show Material materials with Elongation of 13.8 % | Predicted Value, A200 | ||||
15.5 % Show Material materials with Elongation of 15.5 % | Predicted Value, A80 | |||||
17.1 % Show Material materials with Elongation of 17.1 % | Predicted Value, Transverse | |||||
18.7 % Show Material materials with Elongation of 18.7 % | Predicted Value, A80 Transverse | |||||
20.8 % Show Material materials with Elongation of 20.8 % | Predicted Value, A5 | |||||
22.5 % Show Material materials with Elongation of 22.5 % | Predicted Value, A50 | |||||
20 °C | 17 % Show Material materials with Elongation of 17 % | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | ||||
Reduction of area | 40.1 % Show Material materials with Reduction of area of 40.1 % | Predicted Value | ||||
43.9 % Show Material materials with Reduction of area of 43.9 % | Predicted Value, Transverse | |||||
Shear modulus | 79.9 GPa Show Material materials with Shear modulus of 79.9 GPa | Predicted Value | ||||
Shear strength | 591 MPa Show Material materials with Shear strength of 591 MPa | Predicted Value | ||||
Tensile strength | 20 °C | 540 - 770 MPa Show Material materials with Tensile strength of 540 - 770 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | |
20 °C | 540 - 720 MPa Show Material materials with Tensile strength of 540 - 720 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 590 - 770 MPa Show Material materials with Tensile strength of 590 - 770 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 590 - 720 MPa Show Material materials with Tensile strength of 590 - 720 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Yield strength | 310.9 MPa Show Material materials with Yield strength of 310.9 MPa | Predicted Value, RP1 | ||||
331.2 MPa Show Material materials with Yield strength of 331.2 MPa | Predicted Value, RP1 Transverse | |||||
438.1 MPa Show Material materials with Yield strength of 438.1 MPa | Predicted Value, Transverse | |||||
447.9 MPa Show Material materials with Yield strength of 447.9 MPa | Predicted Value, RP02 | |||||
476.8 MPa Show Material materials with Yield strength of 476.8 MPa | Predicted Value, RP02 Transverse | |||||
524.7 MPa Show Material materials with Yield strength of 524.7 MPa | Predicted Value, RP05 | |||||
569.3 MPa Show Material materials with Yield strength of 569.3 MPa | Predicted Value, RP002 | |||||
20 °C | 440 MPa Show Material materials with Yield strength of 440 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 480 MPa Show Material materials with Yield strength of 480 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 500 MPa Show Material materials with Yield strength of 500 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 11.95 1/K Show Material materials with Coefficient of thermal expansion of 11.95 1/K | Predicted Value |
Specific heat capacity | 442.6 J/(kg·K) Show Material materials with Specific heat capacity of 442.6 J/(kg·K) | Predicted Value |
Thermal conductivity | 36.2 W/(m·K) Show Material materials with Thermal conductivity of 36.2 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Boron | 0.005 % Show Material materials with Boron of 0.005 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Carbon | 0.18 % Show Material materials with Carbon of 0.18 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Chromium | 1 % Show Material materials with Chromium of 1 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Copper | 0.3 % Show Material materials with Copper of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Manganese | 1.7 % Show Material materials with Manganese of 1.7 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Molybdenum | 0.7 % Show Material materials with Molybdenum of 0.7 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nickel | 1.5 % Show Material materials with Nickel of 1.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nitrogen | 0.015 % Show Material materials with Nitrogen of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Silicon | 0.6 % Show Material materials with Silicon of 0.6 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Sulfur | 0.005 % Show Material materials with Sulfur of 0.005 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
0.01 % Show Material materials with Sulfur of 0.01 % | quenched and tempered (+QT) | EN 10028-6 | Flat | |
Titanium | 0.05 % Show Material materials with Titanium of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Zirconium | 0.15 % Show Material materials with Zirconium of 0.15 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |