Unclassified Low Alloy Steel
EN 10028-6 Grade P500QL1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QL2 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P500Q quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QH quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10297-1 Grade 36Mn4 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10277-2 Grade St52-3 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade ZSt52-3 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 50-2 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 60-2 cold drawnKohlenstoffarmer Stahl
EN 10277-2 Grade St 70-2 cold drawn