Streckgrenze: 560 MPa

Quick Comparison

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S620Q quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

UNS C18400 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C18150 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C51100 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19000 boway

Geliefert von:

Ningbo Boway Alloy Material

Chromium Molybdenum Steel

Firmodur 7220 QT

Geliefert von:

Deutsche Edelstahlwerke (DEW)

Chromium Molybdenum Steel

Firmodur 7226 QT

Geliefert von:

Deutsche Edelstahlwerke (DEW)

Chromium Molybdenum Steel

Firmodur 7225 QT

Geliefert von:

Deutsche Edelstahlwerke (DEW)

Chromium Molybdenum Steel

Firmodur 7227 QT

Geliefert von:

Deutsche Edelstahlwerke (DEW)