EN 10025-6 Grade S620Q quenched and tempered (+QT)

View all suppliers (2)

Want to keep this datasheet? Save it now in your required format

Description

The tempered and fine grain weldable steel S620Q is used for constructions, such as transport vehicles, lifting and earthmoving machines, load-carrying constructions etc. Lowest application temperature -20 °C.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20 °C

7.84 g/cm³

Show Material materials with Density of 7.84 g/cm³

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

20 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Elongation

12.3 %

Show Material materials with Elongation of 12.3 %

Predicted Value, A80

12.7 %

Show Material materials with Elongation of 12.7 %

Predicted Value, A200

15.9 %

Show Material materials with Elongation of 15.9 %

Predicted Value, Transverse

18.2 %

Show Material materials with Elongation of 18.2 %

Predicted Value, A5

18.4 %

Show Material materials with Elongation of 18.4 %

Predicted Value, A80 Transverse

19.1 %

Show Material materials with Elongation of 19.1 %

Predicted Value, A50

20 °C

15 %

Show Material materials with Elongation of 15 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Reduction of area

40.2 %

Show Material materials with Reduction of area of 40.2 %

Predicted Value

44.7 %

Show Material materials with Reduction of area of 44.7 %

Predicted Value, Transverse

Shear modulus

20 °C

80 GPa

Show Material materials with Shear modulus of 80 GPa

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Shear strength

574 MPa

Show Material materials with Shear strength of 574 MPa

Predicted Value

Tensile strength

20 °C

650 - 890 MPa

Show Material materials with Tensile strength of 650 - 890 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

650 - 830 MPa

Show Material materials with Tensile strength of 650 - 830 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

700 - 890 MPa

Show Material materials with Tensile strength of 700 - 890 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

700 - 830 MPa

Show Material materials with Tensile strength of 700 - 830 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Yield strength

309.6 MPa

Show Material materials with Yield strength of 309.6 MPa

Predicted Value, RP1

329.7 MPa

Show Material materials with Yield strength of 329.7 MPa

Predicted Value, RP1 Transverse

502.7 MPa

Show Material materials with Yield strength of 502.7 MPa

Predicted Value, RP02 Transverse

526.4 MPa

Show Material materials with Yield strength of 526.4 MPa

Predicted Value, Transverse

541.7 MPa

Show Material materials with Yield strength of 541.7 MPa

Predicted Value, RP05

569.5 MPa

Show Material materials with Yield strength of 569.5 MPa

Predicted Value, RP02

629 MPa

Show Material materials with Yield strength of 629 MPa

Predicted Value, RP002

20 °C

560 MPa

Show Material materials with Yield strength of 560 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

580 MPa

Show Material materials with Yield strength of 580 MPa

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

20 °C

600 MPa

Show Material materials with Yield strength of 600 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

620 MPa

Show Material materials with Yield strength of 620 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

100 °C

1.2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.2e-05 1/K

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Specific heat capacity

20 °C

430 J/(kg·K)

Show Material materials with Specific heat capacity of 430 J/(kg·K)

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Thermal conductivity

20 °C

40 W/(m·K)

Show Material materials with Thermal conductivity of 40 W/(m·K)

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Electrical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Electrical conductivity

5 S/m

Show Material materials with Electrical conductivity of 5 S/m

Predicted Value

Electrical resistivity

20 °C

2.6e-07 Ω·m

Show Material materials with Electrical resistivity of 2.6e-07 Ω·m

quenched and tempered (+QT)

EN 10025-6, EN 10137-2

Flat

Chemical properties

PropertyValueConditionRelated StandardsShape

Boron

0.005 %

Show Material materials with Boron of 0.005 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Chromium

1.5 %

Show Material materials with Chromium of 1.5 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Copper

0.5 %

Show Material materials with Copper of 0.5 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Manganese

1.7 %

Show Material materials with Manganese of 1.7 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Molybdenum

0.7 %

Show Material materials with Molybdenum of 0.7 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Nickel

2 %

Show Material materials with Nickel of 2 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Niobium

0.06 %

Show Material materials with Niobium of 0.06 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Nitrogen

0.015 %

Show Material materials with Nitrogen of 0.015 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Phosphorus

0.025 %

Show Material materials with Phosphorus of 0.025 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Vanadium

0.12 %

Show Material materials with Vanadium of 0.12 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Zirconium

0.15 %

Show Material materials with Zirconium of 0.15 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.

Do you have a technical question or need more information about this material?