EN 10025 Grade S355K2G4C as-rolled condition (+AR)

Want to keep this datasheet? Save it now in your required format

Description

S355K2G4C is used for folding, section cold forming and cold drawing grade. The high-tensile fine grained steel is applicable for welding constructions of dynamic load up to -20 °C. Compared to S235J2G3C is achievable a considerable saving of material due to the by 120 MPa higher yield point. The steel shows a by 15% higher resistance to mineral wear due to sliding action in comparison to S235J2G4. Mechanical properties have to comply with EURONORM 164 by arrangement. Max. product thickness amounts 20 mm for folding and 8 mm for cold roll forming grades.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation

20.0 °C

22 %

Show Material materials with Elongation of 22 %

Elongation A80

20.0 °C

14 - 18 %

Show Material materials with Elongation A80 of 14 - 18 %

Elongation A80, transverse

20.0 °C

12 - 16 %

Show Material materials with Elongation A80, transverse of 12 - 16 %

Elongation, transverse

20.0 °C

20 %

Show Material materials with Elongation, transverse of 20 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Shear modulus

23.0 °C

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Tensile strength

20.0 °C

490 - 680 MPa

Show Material materials with Tensile strength of 490 - 680 MPa

Yield strength

20.0 °C

345 - 355 MPa

Show Material materials with Yield strength of 345 - 355 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Max service temperature, long

-20 - 0 °C

Show Material materials with Max service temperature, long of -20 - 0 °C

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

23.0 °C

465 J/(kg·K)

Show Material materials with Specific heat capacity of 465 J/(kg·K)

Typical for Low Carbon Steel

Thermal conductivity

23.0 °C

25 - 93 W/(m·K)

Show Material materials with Thermal conductivity of 25 - 93 W/(m·K)

Typical for Low Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Manganese

1.6 %

Show Material materials with Manganese of 1.6 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.55 %

Show Material materials with Silicon of 0.55 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %