Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Härte, HBW | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, HBW of 270 [-] |
Streckgrenze | 23.0 °C | 450 MPa Show Supplier Material materials with Streckgrenze of 450 MPa |
Zugfestigkeit | 23.0 °C | 650 - 880 MPa Show Supplier Material materials with Zugfestigkeit of 650 - 880 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 21 - 23 % Show Supplier Material materials with Chrom of 21 - 23 % |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 2.5 - 3.5 % Show Supplier Material materials with Molybdän of 2.5 - 3.5 % |
Nickel | 4.5 - 6.5 % Show Supplier Material materials with Nickel of 4.5 - 6.5 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.08 - 0.2 % Show Supplier Material materials with Stickstoff of 0.08 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Oil and gas, Marine |