Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Streckgrenze | 23.0 °C | 600 - 930 MPa Show Supplier Material materials with Streckgrenze of 600 - 930 MPa |
Zugfestigkeit | 23.0 °C | 380 MPa Show Supplier Material materials with Zugfestigkeit of 380 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 17.5 - 19.5 % Show Supplier Material materials with Chrom of 17.5 - 19.5 % |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Nickel | 8 - 10.5 % Show Supplier Material materials with Nickel of 8 - 10.5 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.11 % Show Supplier Material materials with Stickstoff of 0.11 % |
Technological properties
Property | ||
---|---|---|
Application areas | General Engineering |