Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 % Show Supplier Material materials with Dehnung of 12 % |
Härte, HBW | 23.0 °C | 360 [-] Show Supplier Material materials with Härte, HBW of 360 [-] |
Streckgrenze | 23.0 °C | 520 - 1000 MPa Show Supplier Material materials with Streckgrenze of 520 - 1000 MPa |
Zugfestigkeit | 23.0 °C | 800 - 1270 MPa Show Supplier Material materials with Zugfestigkeit of 800 - 1270 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 0.15 - 0.45 % Show Supplier Material materials with Andere of 0.15 - 0.45 % | Nb+Ta |
Chrom | 15 - 17.5 % Show Supplier Material materials with Chrom of 15 - 17.5 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | |
Molybdän | 0.6 % Show Supplier Material materials with Molybdän of 0.6 % | |
Nickel | 3 - 5 % Show Supplier Material materials with Nickel of 3 - 5 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Oil and gas |