Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Härte, HBW | 23.0 °C | 290 [-] Show Supplier Material materials with Härte, HBW of 290 [-] |
Streckgrenze | 23.0 °C | 530 MPa Show Supplier Material materials with Streckgrenze of 530 MPa |
Zugfestigkeit | 23.0 °C | 730 - 930 MPa Show Supplier Material materials with Zugfestigkeit of 730 - 930 MPa |
Chemical properties
Property | Value |
---|---|
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % |
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 1.2 % Show Supplier Material materials with Mangan of 1.2 % |
Molybdän | 3 - 5 % Show Supplier Material materials with Molybdän of 3 - 5 % |
Nickel | 6 - 8 % Show Supplier Material materials with Nickel of 6 - 8 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % |
Silizium | 0.8 % Show Supplier Material materials with Silizium of 0.8 % |
Stickstoff | 0.24 - 0.32 % Show Supplier Material materials with Stickstoff of 0.24 - 0.32 % |
Technological properties
Property | ||
---|---|---|
Application areas | Oil and gas, Marine |