Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 40 % Show Supplier Material materials with Dehnung of 40 % |
Härte, HBW | 23.0 °C | 215 [-] Show Supplier Material materials with Härte, HBW of 215 [-] |
Streckgrenze | 23.0 °C | 200 MPa Show Supplier Material materials with Streckgrenze of 200 MPa |
Zugfestigkeit | 23.0 °C | 500 - 700 MPa Show Supplier Material materials with Zugfestigkeit of 500 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 16.5 - 18.5 % Show Supplier Material materials with Chrom of 16.5 - 18.5 % |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 2 - 2.5 % Show Supplier Material materials with Molybdän of 2 - 2.5 % |
Nickel | 10 - 13 % Show Supplier Material materials with Nickel of 10 - 13 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.11 % Show Supplier Material materials with Stickstoff of 0.11 % |
Technological properties
Property | ||
---|---|---|
Application areas | Precison components, General Engineering |