Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 % Show Supplier Material materials with Dehnung of 12 % |
Streckgrenze | 23.0 °C | 550 MPa Show Supplier Material materials with Streckgrenze of 550 MPa |
Zugfestigkeit | 23.0 °C | 750 - 950 MPa Show Supplier Material materials with Zugfestigkeit of 750 - 950 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 15.5 - 17.5 % Show Supplier Material materials with Chrom of 15.5 - 17.5 % |
Kohlenstoff | 0.33 - 0.45 % Show Supplier Material materials with Kohlenstoff of 0.33 - 0.45 % |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % |
Molybdän | 0.8 - 1.3 % Show Supplier Material materials with Molybdän of 0.8 - 1.3 % |
Nickel | 1 % Show Supplier Material materials with Nickel of 1 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automobile |