Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % |
Streckgrenze | 23.0 °C | 400 MPa Show Supplier Material materials with Streckgrenze of 400 MPa |
Zugfestigkeit | 23.0 °C | 600 - 950 MPa Show Supplier Material materials with Zugfestigkeit of 600 - 950 MPa |
Chemical properties
Property | Value |
---|---|
Andere | 1 % Show Supplier Material materials with Andere of 1 % |
Chrom | 17 - 19 % Show Supplier Material materials with Chrom of 17 - 19 % |
Kohlenstoff | 0.1 % Show Supplier Material materials with Kohlenstoff of 0.1 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Nickel | 8 - 10 % Show Supplier Material materials with Nickel of 8 - 10 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.15 - 0.35 % Show Supplier Material materials with Schwefel of 0.15 - 0.35 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.11 % Show Supplier Material materials with Stickstoff of 0.11 % |
Technological properties
Property | ||
---|---|---|
Application areas | Precison components |