Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.26 g/cm³ Show Supplier Material materials with Dichte of 8.26 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 2 % Show Supplier Material materials with Dehnung A5 of 2 % | |
Elastizitätsmodul | 23.0 °C | 126 GPa Show Supplier Material materials with Elastizitätsmodul of 126 GPa | |
Härte, HBW | 23.0 °C | 320 [-] Show Supplier Material materials with Härte, HBW of 320 [-] | HBW 10/3000 |
Härte, Rockwell C | 23.0 °C | 33 [-] Show Supplier Material materials with Härte, Rockwell C of 33 [-] | |
Streckgrenze Rp0,5 | 23.0 °C | 586 MPa Show Supplier Material materials with Streckgrenze Rp0,5 of 586 MPa | |
Zugfestigkeit | 23.0 °C | 830 MPa Show Supplier Material materials with Zugfestigkeit of 830 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 106 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 106 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.16E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.16E+7 S/m |
Specific Electrical conductivity | 20 % IACS Show Supplier Material materials with Specific Electrical conductivity of 20 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | ||
Beryllium | 2 % Show Supplier Material materials with Beryllium of 2 % | ||
Kobalt | 0.5 % Show Supplier Material materials with Kobalt of 0.5 % | Co+Ni | |
Kupfer | Balance | ||
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % | Co+Ni |
Technological properties
Property | ||
---|---|---|
Application areas | 2.1247 is used wherever good wear resistance or high mechanical properties are desired coupled with a good electrical or thermal conductivity, such as: Flash butt welding and butt welding, Parts for electrical components, in the plastic mould industry is sometimes used as chill plates and inserts in the moulds, cooling pins and neck rings or bottom plates for blow moulds of plastic bottles. |