Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 47 % Show Supplier Material materials with Dehnung of 47 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 53 % Show Supplier Material materials with Flächenreduzierung of 53 % | |
Härte, Brinell | 23.0 °C | 125 [-] Show Supplier Material materials with Härte, Brinell of 125 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 193 MPa Show Supplier Material materials with Streckgrenze of 193 MPa | |
Zugfestigkeit | 23.0 °C | 469 MPa Show Supplier Material materials with Zugfestigkeit of 469 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 6 - 8.5 % Show Supplier Material materials with Aluminium of 6 - 8.5 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Kupfer | Balance, including silver | ||
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Tube sheets,pickling hooks,impellers,valve seats,chemical plants,pulp mills |