Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 28 % Show Supplier Material materials with Dehnung of 28 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 28 % Show Supplier Material materials with Flächenreduzierung of 28 % | |
Härte, Brinell | 23.0 °C | 140 [-] Show Supplier Material materials with Härte, Brinell of 140 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 241 MPa Show Supplier Material materials with Streckgrenze of 241 MPa | |
Zugfestigkeit | 23.0 °C | 545 MPa Show Supplier Material materials with Zugfestigkeit of 545 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 8.5 - 11 % Show Supplier Material materials with Aluminium of 8.5 - 11 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 0.5 - 1.5 % Show Supplier Material materials with Eisen of 0.5 - 1.5 % | ||
Kupfer | Balance, including silver | ||
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Cast iron, Cast iron, Malleable iron, Cast iron to steel, Cast iron to bronze, Steel to bronze, Aluminum bronze, Silicon bronze, Manganese bronze, Cupro-nickel, Copper to steel, Bearings, Bushings, Pump housings, Condenser boxes, Hydraulic pistons, Brake drums, Tractor gear housings, Idler pulleys, Pickling hooks, Paper mill rolls, Motor bases, Tin plate mill rolls, Impellers, Valve seats, Gears, Mixer arms, Press rams, Ship propellers, Lance heads |