Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 27 % Show Supplier Material materials with Dehnung of 27 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 38 % Show Supplier Material materials with Flächenreduzierung of 38 % | |
Härte, Brinell | 23.0 °C | 185 [-] Show Supplier Material materials with Härte, Brinell of 185 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 386 MPa Show Supplier Material materials with Streckgrenze of 386 MPa | |
Zugfestigkeit | 23.0 °C | 655 MPa Show Supplier Material materials with Zugfestigkeit of 655 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 7 - 8.5 % Show Supplier Material materials with Aluminium of 7 - 8.5 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 2 - 4 % Show Supplier Material materials with Eisen of 2 - 4 % | ||
Kupfer | Balance, including silver | ||
Mangan | 11 - 14 % Show Supplier Material materials with Mangan of 11 - 14 % | ||
Nickel | 1.5 - 3 % Show Supplier Material materials with Nickel of 1.5 - 3 % | ||
Silizium | 1.5 % Show Supplier Material materials with Silizium of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Ship propellers, Marine components, Welding cast iron, Joining dissimilar metals |