Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 22 % Show Supplier Material materials with Flächenreduzierung of 22 % | |
Härte, Brinell | 23.0 °C | 187 [-] Show Supplier Material materials with Härte, Brinell of 187 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 400 MPa Show Supplier Material materials with Streckgrenze of 400 MPa | |
Zugfestigkeit | 23.0 °C | 683 MPa Show Supplier Material materials with Zugfestigkeit of 683 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 8.5 - 9.5 % Show Supplier Material materials with Aluminium of 8.5 - 9.5 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 3 - 6 % Show Supplier Material materials with Eisen of 3 - 6 % | ||
Kupfer | Balance, including silver | ||
Mangan | 0.5 - 3.5 % Show Supplier Material materials with Mangan of 0.5 - 3.5 % | ||
Nickel | 4 - 6 % Show Supplier Material materials with Nickel of 4 - 6 % | ||
Silizium | 1.5 % Show Supplier Material materials with Silizium of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Ship fittings, Propeller gear housings, Power plant valves, Marine propulsion systems, Intake screens, Ship propellers, Welding AMPCO® 45, Piping systems, Welding AMPCO® 483, Oil recovery pumps |