Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 22 % Show Supplier Material materials with Flächenreduzierung of 22 % | |
Härte, Brinell | 23.0 °C | 166 [-] Show Supplier Material materials with Härte, Brinell of 166 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 276 MPa Show Supplier Material materials with Streckgrenze of 276 MPa | |
Zugfestigkeit | 23.0 °C | 621 MPa Show Supplier Material materials with Zugfestigkeit of 621 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 10 - 11.5 % Show Supplier Material materials with Aluminium of 10 - 11.5 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 2 - 4.5 % Show Supplier Material materials with Eisen of 2 - 4.5 % | ||
Kupfer | Balance, including silver | ||
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Hydraulic pistons, Bearing overlays, Impellers, Turbine runners, Press rams, Cable sheaves, Mill slippers, Valve seats and parts, Breaker blocks, Ceiling machine mandrels, Steel mill rolls, Welding AMPCO® 18 |