Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 17 % Show Supplier Material materials with Flächenreduzierung of 17 % | |
Härte, Brinell | 23.0 °C | 160 [-] Show Supplier Material materials with Härte, Brinell of 160 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 324 MPa Show Supplier Material materials with Streckgrenze of 324 MPa | |
Zugfestigkeit | 23.0 °C | 614 MPa Show Supplier Material materials with Zugfestigkeit of 614 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 9.5 - 11.5 % Show Supplier Material materials with Aluminium of 9.5 - 11.5 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 2.5 - 5 % Show Supplier Material materials with Eisen of 2.5 - 5 % | ||
Kupfer | Balance, including silver | ||
Silizium | 1.5 % Show Supplier Material materials with Silizium of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Bronze castings, Strip mill guides, Bearing overlays, Crane contact shoes, Driving sprockets, Drop hammers, Manipulator slides, Gate valves, Sheaves, Pistons, Mill slippers, Turbine runners, Packing glands, Valve seat overlays |