Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 0 % Show Supplier Material materials with Dehnung of 0 % | in 2″ (51 mm) |
Härte, Brinell | 23.0 °C | 340 [-] Show Supplier Material materials with Härte, Brinell of 340 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 386 MPa Show Supplier Material materials with Streckgrenze of 386 MPa | |
Zugfestigkeit | 23.0 °C | 538 MPa Show Supplier Material materials with Zugfestigkeit of 538 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 13 - 14 % Show Supplier Material materials with Aluminium of 13 - 14 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 3 - 5 % Show Supplier Material materials with Eisen of 3 - 5 % | ||
Kupfer | Balance, including silver | ||
Silizium | 0.04 % Show Supplier Material materials with Silizium of 0.04 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Wear shoes, Chafing plates, Clutch fingers, Screw conveyors, Forming dies, Sleeves, Cams, Welding AMPCO® 22 |