Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 0 % Show Supplier Material materials with Dehnung of 0 % | in 2″ (51 mm) |
Härte, Brinell | 23.0 °C | 370 [-] Show Supplier Material materials with Härte, Brinell of 370 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 476 MPa Show Supplier Material materials with Streckgrenze of 476 MPa | |
Zugfestigkeit | 23.0 °C | 558 MPa Show Supplier Material materials with Zugfestigkeit of 558 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 14 - 15 % Show Supplier Material materials with Aluminium of 14 - 15 % | ||
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Eisen | 3 - 5 % Show Supplier Material materials with Eisen of 3 - 5 % | ||
Kupfer | Balance, including silver | ||
Silizium | 0.04 % Show Supplier Material materials with Silizium of 0.04 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Draw dies, Wear shoes, Wear strips, Slides, Forming dies, Wear plates, Cams, Welding AMPCO® 25 |