Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
AMPCO-TRODE® 940
AMPCO-TRODE® 940 is an alloy developed to provide an effective alternative to beryllium copper. One of its principal applications is for molds and mold components in the plastics industry. Because of its excellent thermal conductivity, thermal diffusivity, wear resistance and corrosion resistance, AMPCO-TRODE® 940 filler metal is specified for the repair of complex AMPCOLOY® 940 molds used in forming plastic parts.
AMPCO-TRODE® 940 is applied with the gas tungsten-arc welding processes.
Diese Materialdaten wurden von AMPCO METAL zur Verfügung gestellt
All categories
AMPCOLOY® 940: Beryllium-Free Copper Alloy for the Plastic Industry
Aluminium Bronze Alloys by AMPCO METAL: The finest materials for deep drawing tools
Choosing the Right Welding Process: GMAW vs TIG vs SMAW vs FCAW
Tool Materials for Metal Forming: The Case for Aluminium Bronze
Weld Spatter and How Anti-Spatter Materials Can Minimise it
What Filler Metal to Use in Welding Dissimilar Metals?
Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Chrom | 0.1 - 0.6 % Show Supplier Material materials with Chrom of 0.1 - 0.6 % | ||
Kupfer | Balance, including silver | ||
Nickel | 2 - 3 % Show Supplier Material materials with Nickel of 2 - 3 % | ||
Silizium | 0.4 - 0.8 % Show Supplier Material materials with Silizium of 0.4 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Mold cores and pins, Repair of blow molds, Injection molds |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.