Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Chrom | 0.1 - 0.6 % Show Supplier Material materials with Chrom of 0.1 - 0.6 % | ||
Kupfer | Balance, including silver | ||
Nickel | 2 - 3 % Show Supplier Material materials with Nickel of 2 - 3 % | ||
Silizium | 0.4 - 0.8 % Show Supplier Material materials with Silizium of 0.4 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Repair of blow molds, injections molds, Their components, such as cores and pins, Made in AMPCOLOY® 940 | |
Other | AMPCO-TRODE® 940 laser filler metal is available from stock in the following diameters: 0.25, 0.3, 0.4, and 0.5 mm. Other larger diameters are available upon request. | |
Processing methods | Shielding gas: 100% Argon Gas flow rate: 8-12 L/min, depending on nozzle diameter |