Allgemein
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 29 % Show Supplier Material materials with Dehnung of 29 % | in 2″ (51 mm) |
Flächenreduzierung | 23.0 °C | 45 % Show Supplier Material materials with Flächenreduzierung of 45 % | |
Härte, Brinell | 23.0 °C | 54 [-] Show Supplier Material materials with Härte, Brinell of 54 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Streckgrenze | 23.0 °C | 55 MPa Show Supplier Material materials with Streckgrenze of 55 MPa | |
Zugfestigkeit | 23.0 °C | 200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 40 % IACS Show Supplier Material materials with Specific Electrical conductivity of 40 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | max. | |
Kupfer | Balance, including silver | ||
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Phosphor | 0.15 % Show Supplier Material materials with Phosphor of 0.15 % | max. | |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. | |
Zinn | 1 % Show Supplier Material materials with Zinn of 1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Billet molds, Conductor rolls, Heater elements, Copper sculptures, Steel mill electrode holders, Bus bars, Copper connectors |