Copper Nickel 90/10 Copper Alloy

View suppliers (7)
Want to keep this datasheet? Save it now in your required format

Description

2.0872 (CuNi10Fe1Mn) cupronickel is a 90% copper, 10% nickel alloy that also contains small but important additions of iron and manganese to enhance overall strength corrosion resistance. This, combined with high ductility and toughness, makes it a popular grade for marine, architectural and industrial applications. It shows the following features and properties:


  • High ductility and toughness
  • Excellent resistance to erosion and corrosion in seawater
  • Inherent resistance to biofouling
  • Excellent fabrication and welding properties
  • Retention of mechanical properties down to cryogenic temperatures
  • Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    27 - 30 %

    Show Material materials with Dehnung of 27 - 30 %

    Härte, Brinell

    23.0 °C

    70 - 120 [-]

    Show Material materials with Härte, Brinell of 70 - 120 [-]

    Streckgrenze Rp 0,2

    23.0 °C

    105 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 105 MPa

    Zugfestigkeit

    23.0 °C

    280 - 310 MPa

    Show Material materials with Zugfestigkeit of 280 - 310 MPa

    Chemical properties

    PropertyValue

    Eisen

    1.5 %

    Show Material materials with Eisen of 1.5 %

    Kupfer

    Balance

    Mangan

    0.75 %

    Show Material materials with Mangan of 0.75 %

    Nickel

    10.5 %

    Show Material materials with Nickel of 10.5 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Salt water pipes and fittings, hot water tanks, salt water baffles, propeller sleeves, valve and pump components, flanges, boat hulls, marine fittings and marine hardware;Chemical processing: Heat exchanger and cooling plant, evaporator tubes, pump and valve trim;Other: Power steering tube, brake lines, condenser plates, pressure vessels and distiller tubes

    Corrosion properties

    Excellent resistance to erosion and corrosion in seawater.

    General machinability

    Easily machined