1.4980 (X6NiCrTiMoVB25-15-2) is special corrosion, oxidation and heat resistant, precipitation hardenable austenitic stainless steel. It is designed for long-term, high strength service up to 700°C. It is non-magnetic even after severe cold deformation. The alloy has good oxidation resistance in continuous service up to 800°C. It shows the following features and properties:


  • Very high corrosion resistance
  • Good oxidation resistance up to 800°C
  • Non-magnetic even after severe cold deformation
  • High strengths that are well retained up to 700°C
  • Good machinability
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Mechanisch

    PropertyTemperatureValueComment

    Dehnung

    23.0 °C

    15 %

    Show Material materials with Dehnung of 15 %

    Härte, Brinell

    23.0 °C

    248 [-]

    Show Material materials with Härte, Brinell of 248 [-]

    max.

    Streckgrenze

    23.0 °C

    585 MPa

    Show Material materials with Streckgrenze of 585 MPa

    Zugfestigkeit

    23.0 °C

    895 MPa

    Show Material materials with Zugfestigkeit of 895 MPa

    Chemical properties

    PropertyValue

    Chrom

    15 %

    Show Material materials with Chrom of 15 %

    Eisen

    56 %

    Show Material materials with Eisen of 56 %

    Molybdän

    1.5 %

    Show Material materials with Molybdän of 1.5 %

    Nickel

    25.5 %

    Show Material materials with Nickel of 25.5 %

    Titan

    2.1 %

    Show Material materials with Titan of 2.1 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Fasteners, and critical pump/valve components;Aerospace: Turbine shafts, aero engine components and high performance fasteners;Power generation: Components for gas turbines, turbine discs, and turbine blades;Other: Springs, screws, bolts, thrust nozzles and transmission parts

    Corrosion properties

    Very high corrosion resistance

    General machinability

    It has good machinability and machines best in the precipitation-hardened condition when it has a machinability rating 45% that of AISI1212 free-cutting grade.