Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.05 GPa Show Supplier Material materials with Elastizitätsmodul of 0.05 GPa | dry | ISO 527-1/-2 | |
Härte, Shore A | 92 [-] Show Supplier Material materials with Härte, Shore A of 92 [-] | dry | ISO 868 | 3s |
Härte, Shore D | 33 [-] Show Supplier Material materials with Härte, Shore D of 33 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 18 MPa Show Supplier Material materials with Zugfestigkeit of 18 MPa | dry | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 33 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 33 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |